Microstructural Evolution of Composite 8 WC-(Co, Ni): Effect of the addition of SiC

dc.contributor.authorMiranda F.
dc.contributor.authorRodrigues D.
dc.contributor.authorNakamoto F.Y.
dc.contributor.authorFrajuca C.
dc.contributor.authorSantos G.A.D.
dc.contributor.authorCouto A.A.
dc.date.accessioned2024-03-13T00:54:51Z
dc.date.available2024-03-13T00:54:51Z
dc.date.issued2016
dc.description.abstract© 2016 Trans Tech Publications, Switzerland.Tungsten carbide (WC) based cemented carbides, also called hardmetals, are a family of composite materials consisting of carbide ceramic particles embedded in a metallic binder. They are classified as metal matrix composites (MMCs) because the metallic binder is the matrix that holds the bulk material together [1]. WC based composites are used in applications where a good combination of hardness and toughness are necessary [2]. It is usual to add more components to tailor the microstructure of the WC-(Co, Ni) system. The hardness for the cemented carbides based on nickel, increases significantly because of the addition of reinforcements like SiC nano-whisker [3]. In this work, the SiC was considered as an additional component for the composite WC-8(Co, Ni). Four mixtures were prepared with SiC contents ranging from 0 to 3.0 wt%. These mixtures were pressed (200 MPa) and green samples with 25.2 mm of diameter and 40 g were produced. Sintering was carried out in Sinter-HIP furnace (20 bar). Two sintering temperatures were investigated, i.e. 1380 and 1420°C, and the sintering time considered was 60 minutes. The relative density, hardness, linear and volumetric shrinkage were determined. Microstructural evaluation was investigated by optical microscopy and scanning electron microscopy (SEM-FEG). The results showed that the addition of SiC promoted higher densification and grain size growth. The hardness was higher for samples with SiC, so solid solution hardening of the binder was more effective than WC grain size growth.
dc.description.firstpage78
dc.description.lastpage85
dc.description.volume371
dc.identifier.doi10.4028/www.scientific.net/DDF.371.78
dc.identifier.issn1662-9507
dc.identifier.urihttps://dspace.mackenzie.br/handle/10899/36065
dc.relation.ispartofDefect and Diffusion Forum
dc.rightsAcesso Restrito
dc.subject.otherlanguageComposite
dc.subject.otherlanguageHardmetal
dc.subject.otherlanguageMicrostructural characterization
dc.subject.otherlanguageNi)
dc.subject.otherlanguageSiC
dc.subject.otherlanguageSintering
dc.subject.otherlanguageWC-8(Co
dc.titleMicrostructural Evolution of Composite 8 WC-(Co, Ni): Effect of the addition of SiC
dc.typeArtigo
local.scopus.citations11
local.scopus.eid2-s2.0-85014054101
local.scopus.subjectCarbide ceramics
local.scopus.subjectCemented carbides
local.scopus.subjectHard metals
local.scopus.subjectMicro-structural characterization
local.scopus.subjectMicrostructural evaluation
local.scopus.subjectSintering temperatures
local.scopus.subjectSolid solution hardening
local.scopus.subjectVolumetric shrinkage